Appearance | White powder |
Thickening time, min/65 ℃,35MPa,30min | ≤120 |
Expansion ratio (﹪), Plastic state(75℃, 0.1MPa) | ≥0.10 |
Expansion ratio (﹪),Cementation station (75℃, 0.1MPa,24h) | 0.01≤Ex-Ex0≤0.8 |
Compression strength, MPa/75 ℃, 0.1MPa,24h | ≥14 |
No.1 The experimental conditions: G class: cement, W/C: 0.44; Water quality: distilled water; Dosage SRC-107 : 2.0﹪ (BWOC). No.2 The plastic state’ expansion ratio is the cement slurry initial set’ expansion ratio. No.3 Ex0:Expansion ratio (the cement slurry without SRC-107), Ex:Expansion ratio (the cement slurry with SRC-107 ). |